MECHANICAL PROPERTIES OF THE DEGRADABLE CHAIN-EXPANDED PLA POLYMER
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    Abstract:

    Objective To study the factors influencing the mechanical properties of the degradable chain expanded PLA polymer. Methods Using GB 9641 88 to make the chain expanded PLA polymer into dumbbell shaped samples , the tensile strength was tested at a speed of 5mm/min by a universal testing machine of high polymer under different conditions of temperature ,time, molecular weight of chain expanding agent , PLA and PCL.Results In the course of chain expanding reaction the mixing temperature , mixing period , curing temperature , curing period , the molecular weight of the chain expand agent , the cross linking agent and PLA each had an influence on the tensile strength of the chain expanding PLA polymer. Conclusion The maximum tensile strength was 24.47 MPa when the ratio of PLA to PCL period equaled to 1∶4 , mixing temperature was 100°C , mixing period was 4min , curing temperature was 130°C , curing period was 6h , the molecular weight of chain expanding agent A , cross-linking agent 1 and PLA.

    参考文献
    相似文献
    引证文献
引用本文

史晓林,戴尅戎,王洪志,汤亭亭.可降解扩链PLA聚合物拉伸强度的研究[J].医用生物力学,2003,18(2):102-106

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期:
  • 出版日期:
关闭